Compression failure is usually a specification problem before it ever becomes a transport problem. A carton that carries a stack of four in a dry warehouse can buckle under a stack of ten in a humid container. This is a specification article: what to write into the order so the factory knows what to build and both sides know what will be measured.
Edge crush and box compression are different numbers
The edge crush test loads a small specimen of combined board on its edge and reports the load the board carries before it fails. It is a material property. The box compression test loads a finished, closed box through its top face and reports the vertical load the whole package carries. It is a package property, because it also depends on the box footprint, the height, the score lines and how the board was converted.
Specify edge crush values when you buy board to a material standard. Specify box compression when you buy a performance guarantee for a finished carton. Buyers shipping into a distribution centre, where cartons sit under a full pallet stack, normally mean box compression.
The test methods to name in the order
A figure without a method is an argument waiting to happen. Name the method and the conditioning in the purchase order:
- Edge crush test — the TAPPI test-method family for the edgewise compression of corrugated board, and the equivalent ISO method for corrugated fibreboard.
- Box compression test — measured on the finished package; ISO 12048 covers compression and stacking of complete, filled transport packages using one apparatus.
- Conditioning — the temperature and relative humidity the samples are held at before testing, and how long they are held there.
- Sample size — how many boxes are tested and whether the reported result is the mean of the set or the lowest unit in it.
Method texts are published by the standards bodies and by the technical association for the pulp, paper and corrugated industries; the TAPPI standards and test methods library is the reference for the edge crush family, and ISO 12048 for compression and stacking of filled packages.
Flute direction and board combination drive the result
Corrugated board carries its useful compression load along the flutes. Flutes running vertically around the walls of a carton support the stack; flutes running horizontally carry very little and let the panels bow. State the flute direction on the dieline and check the first article, because a rotated sheet is invisible on a printed sample.
Board combination matters more than caliper alone. Liner grade, fluting medium and the number of walls set the edge crush value, and a heavier single wall with a light double wall can land in the same compression range while behaving differently once the humidity rises. Ask the supplier for the edge crush value of the exact combination, not for a generic grade name.
Pallet patterns change the load a single carton feels
Column stacking, where every carton sits directly on the carton below, sends the load straight down the walls. It gives the best compression performance and the weakest load stability. Interlocked or brick stacking, where each layer is rotated, ties the pallet together but makes every carton bridge the seams beneath it, so a carton can end up carrying the weight of two rows above instead of one. Overhang beyond the pallet deck adds bending, and a flexible deck lets the whole stack deflect.
Write the intended pattern into the order and test the pallet as built, not as drawn. If the customer or the retailer prescribes a pattern, that prescription becomes part of the compression requirement.
Stacking height and humidity belong in the purchase order
Two assumptions decide whether the specified figure is realistic, so put both in writing:
- Stacking height — how many cartons to a pallet, how many pallets high in the container and in the warehouse, and how long the goods stay stacked.
- Humidity — the moisture the board will pick up on the route. Board loses a large part of its compression strength as moisture content rises, so a figure measured in a temperate laboratory is optimistic for a container crossing the tropics.
State the conditioning atmosphere you want the figure quoted at, and state it as an assumption both sides accept. When a claim is disputed later, the question is always which climate the figure was measured in.
Agree a sample-based acceptance rule
A single average figure is a target, not an acceptance rule. Fix the rule in the order before production:
- the number of boxes tested per batch and how they are drawn from the run;
- the conditioning applied before testing;
- the acceptance value, how many units may fall below it, and the value at which the batch fails outright;
- the action on failure — retest on a doubled sample, or hold the batch;
- who tests: your laboratory, the factory's, or an independent one;
- a sealed reference sample kept by both sides, plus the dimensions and flute direction of the approved first article.
Review the structures built on the products page, see how a custom structure is developed, or contact us to turn a sea-freight route into a compression specification.
Frequently asked questions
Do I need both an edge crush value and a box compression value?
Not always. Edge crush specifies the board; box compression specifies how the finished carton performs under a stack. If you are buying a performance guarantee for a sea-freight route, ask for box compression and let the supplier choose the board combination.
Why does the pallet pattern matter to a single carton?
With column stacking every carton passes load straight to the one below. With interlocked stacking each carton bridges the seams beneath it, so it may carry the weight of two rows above rather than one, and the compression requirement rises.
How many boxes should be tested per batch?
Agree the sample size before production and write it into the order. A workable approach is to test a small group per batch, treat the mean as the reference, hold a stated minimum for every unit, and retest on a doubled sample if the first result falls short.